Glass breakage in large glass-glass modules without external influence

Glass breakage in large glass-glass modules without external influence

If the front or back glass of a PV module breaks a few months after installation, although neither hail nor a visible impact preceded it, the cause is rarely in a single component. In modern, large-format glass-glass modules, glass quality, module size, frame, embedding, mounting, and substructure interact. The term spontaneous glass breakage therefore describes the damage pattern, not yet the cause.

 

This distinction is important for operators. A broken module can still deliver power immediately. Nevertheless, the mechanical integrity, moisture protection, and possibly electrical safety are impaired. A pure yield control is therefore not sufficient. The damage should be documented, professionally assessed, and clearly demarcated from the manufacturer, supplier, EPC, and, if applicable, insurers.

 

The contribution of SecondSol Glass fracture offers a basic classification of external causes, visible features, and possible consequences. This contribution further elaborates on the delayed fracture of large glass-glass modules without an unambiguously recognizable single event.

What is meant by spontaneous glass breakage?

Fractures of the front or back glass are referred to as breaks caused by spontaneous glass breakage, for which no obvious external force such as hail, falling debris, or a falling object is recognizable at the time of discovery. They often occur only after commissioning. However, this does not mean that the glass was broken without a physical cause.

 

Microscopic edge damage, an unfavorable pre-tensioning of the glass, local clamping or contact points, stresses from the frame and embedding as well as the actual storage on the substructure can remain inconspicuous for a long time. Temperature changes, wind loads, and repeated deformation during operation can allow existing weaknesses to grow up to the point of fracture afterwards.

Why modern glass modules are particularly noteworthy

Module designs have changed significantly in a short time. Many new power plant modules are larger than previous generations, have glass on the front and back sides, and frequently use panes of about 2.0 millimeters or less. At the same time, frames and other materials have been optimized in the competition for weight and cost. Each individual change can be technically manageable. However, in their combination, they change the mechanical reserves of the entire module.

 

The IEA Photovoltaic Power Systems Programme indicates that in individual documented projects with thin-film modules, fracture rates of 5 to 10 percent occurred within the first two years of operation. A particularly striking published test was even higher. These cases are warning signs, but not a general failure rate for glass-glass modules. The IEA report expressly emphasizes that the large majority of systems with thin-film modules do not show noticeable glass fracture rates.

Which causes are in question

Causes Possible Mechanism Inspection sample
Glass and frames Low surface tension, edge defects, scratches, or pre-damage reduce the fracture reserve. Inspect the origin, edges, and damages; special measurement of the surface tension only in the laboratory.
Module design A large area, thin glass, and low frame height increase deformation or transmit local forces unfavorably. Compare data sheet, frame geometry, glass thickness, and tested installation configuration.
Frame and mounting Contact between glass and frame, uneven silicone or local pinching creates voltage spikes. Analyze the frame, sealant, contact points, and recurring fracture positions.
Substructure The clamping areas, rail distances, tolerances, or tracker movements do not sufficiently match the module. Compare the installation with the manufacturer's approval and installation instructions.
Transport and installation Subtle edge or surface damage only worsens during operation. Check packaging, handling, site documentation, and serial accumulation.
Operating loads Wind, snow, and temperature changes cyclically stress an already damaged or poorly positioned module. Document the time, weather history, and location of the affected modules.

Thin glass is not automatically defective.

A small glass thickness alone does not prove a product defect. A 2026 study published by the National Laboratory of the Rockies shows that 2.0-millimeter glass can be fully thermally pre-stressed. However, among eleven modules from six solar locations, a statistical correlation was found between lower surface pressure and a higher susceptibility to spontaneous glass fracture. Furthermore, a larger module area correlated with lower surface pressure.

 

The sample size is too small to derive a general market share or a simple threshold rule from it. The authors emphasize that several factors interact. The fracture pattern alone does not allow for a reliable statement about how much the glass was thermally pre-stressed.

Frames and mounting can generate local voltage surges

Kiwa PVEL describes the Mechanical Stress Sequence 2026 glass fracture as a continuing reliability risk. In 26 percent of the bill of materials tested in this series, the so-called Bills of Materials, at least one of the tested modules broke. For 62 percent of the broken test samples, the laboratory found indications of a local pinching of the glass. For modules with an area of 2.5 to 3.0 square meters, the observed fracture rate for frames under 35 millimeters was higher in this test data set than for stronger frames.

 

These values originate from a stricter product qualification program with modules submitted by manufacturers. They are not the failure rate of the entire market and must not be applied to a specific system without examination. For procurement and cause analysis, they still show why the module, frame, sealant, and mounting system should be considered as a common mechanical unit.

Why the IEC type testing does not detect every vulnerability

The construction approval according to IEC 61215 includes mechanical load tests. It is an important minimum requirement, but it does not answer every project-specific reliability question. Glass breakage is a statistical event: A small number of successful test samples can overlook a risk that occurs only in a part of a batch or in a specific mounting configuration.

 

The IEA PVPS therefore recommends an examination of approximately 20 modules of one type in the final installation position for the rough assessment of thin glass-glass modules. This allows the fracture rate in the range of approximately 5 percent to be roughly assessed. This is not a general legal obligation but a professional recommendation for a more reliable risk assessment.

How operators recognize and document glass breakage

Front glass breakage is often visible. Back glass breakage can remain undetected for a long time in roof systems, densely packed module fields, or low ground clearance. Monitoring data also only help to a limited extent because a module can still show an inconspicuous electrical output immediately after the break.

 

In case of an abnormality, operators and O&M companies should document at least:

  • Installation area, table, string, and exact module position
  • Manufacturer, module type, serial number, batch, and delivery date
  • Front glass, back glass, or both sides as well as the recognizable fracture origin
  • Recurring fracture points, for example at the center of the frame, corner, clamp, or support point
  • Installation method, clamping area, rail spacing, torque requirements, and substructure
  • Time of discovery and known wind, snow, hail, or temperature events
  • Photos from several perspectives and, if safe, detailed images of the frame and edges
  • Electrical abnormalities, insulation alarms, and previous test results

Work in the generator field, electrical measurements, and the dismantling of damaged modules belong in the hands of qualified specialists. Especially when the backsheet is broken, a safe visual inspection is not possible in every installation situation.

Which checks are meaningful in a series of damage

For a single obvious transport damage, replacement is sufficient. If several breaks of the same type or in comparable positions occur, the investigation should be systematically expanded. The goal is not only to find damaged modules but to recognize a recurring pattern and the probable load path.

  • Structured visual inspection of the affected field and a defined comparison sample
  • Comparison of the installation with module and substructure approvals
  • Control of clamps, rails, frame contact, tolerances, and possible forced situations
  • Insulation measurement and further electrical safety check by an electrical specialist
  • Characteristic curve measurement if power and string behavior need to be assessed
  • Electroluminescence if additional cell cracks or mechanical consequential damage are to be investigated
  • Laboratory analysis of the fracture origin or the glass surface tension in disputed series cases

An electroluminescence testing can reveal cell damage, but it does not automatically explain the cause of the glass fracture. Conversely, a seemingly unremarkable power measurement does not rule out a safety-relevant glass damage. The contribution Fault patterns insulation faults in PV systems also contains information on systematically limiting electrical abnormalities.

Continued operation Repair or replacement

Broken module glass cannot generally be permanently and manufacturer-compliant repaired in the field. Provisional coatings or adhesives do not reliably restore the original mechanical strength, electrical insulation, and long-term sealing. For grid-tied systems, therefore, the proper replacement is regularly the appropriate solution.

 

Before the decision on replacement, an electrical expert should assess whether the affected part of the system can continue to be operated or must be taken out of service. Factors include, among others, the extent of the break, the installation situation, moisture, insulation values, manufacturer specifications, and the risk of falling parts. A continued normal yield is not sufficient proof of release.

What the operator should consider in case of complaint and procurement

In case of a large quantity, the documentation should be sent to the manufacturer, supplier, EPC, and where applicable, the insurers at an early stage. In addition to the broken modules, it must be noted how many identical modules are still intact. Only in this way can the scale of a possible series be assessed. Before extensive dismantling, it must be agreed which modules or fragments need to be secured for a cause analysis.

 

For new projects or spare parts procurement, in addition to the data sheet and warranty, the following questions are particularly helpful:

  • Which specific bill of materials was independently checked and does it correspond to the delivered version?
  • What glass thicknesses, frame dimensions, and sealing systems are used?
  • In which installation configuration were mechanical load tests performed?
  • Is the combination of module and substructure or tracker expressly approved?
  • Are there extended Mechanical Stress Sequence results or project-specific spot checks?
  • How are serial numbers, batches, and changes to the bill of materials documented?
  • What reaction and proof obligations apply in the event of a warranty claim?

Organize spare modules and spare parts logistics proactively

When replacing individual modules, it is not sufficient to choose only a similar power class. Dimensions, electrical characteristics, connection system, maximum system voltage, current load capacity, and integration into the existing string must all be compatible. Especially for older or no longer produced module types, a compatible replacement module can be more economical than refitting an entire field.

Marketplace and own spare parts inventory

On the SecondSol Marketplace, operators, installers, and O&M companies can search for new, used, or refurbished spare components. The offers available there do not only come from external market participants: SecondSol itself holds a large inventory of photovoltaic spare parts. According to the current company status, there are more than 250,000 parts in stock; in addition, there are further offers from the European SecondSol network.

 

This is particularly relevant for existing installations because manufacturers and wholesalers no longer regularly supply certain module series after just a few years. An existing old stock, a tested used module, or a technically suitable replacement module can then help to remedy individual damages without refitting an entire module field. Whether a replacement module fits must be checked based on the mechanical and electrical data as well as the specific string design.

Project-based stockpiling for professional operators

For large solar parks and commercial portfolios, the question of spare parts should not begin only after the next glass breakage. A defined reserve of identical or approved spare modules can be provided during construction, repowering, or a larger replacement procurement. The required quantity depends, among other things, on the system size, module type, failure history, recovery risk, and agreed response time.

 

SecondSol can take over such customer-owned spare parts inventories as part of its Photovoltaic Fulfillment Service. This includes the storage of PV modules and other spare parts, unambiguous inventory assignment, stock maintenance, picking, and shipping as needed. If an operator requires replacement modules for a specific incident, the intended components can be provided regularly, by express, or as direct shipment and, if desired, delivered just-in-time to the construction site.

 

This turns a one-time spare parts search into a predictable process: determine suitable modules, store a reserve stock, document withdrawals, and deliver the required quantities to the intended location. For operators of multiple systems, inventories can also be assigned to specific parks, module types, or service contracts. This reduces search times in case of a fault and prevents the need to procure rare compatible modules under time pressure.

Do not store glass breakage modules as spare parts

Damaged glass modules are not regular reusable spare parts. Before transport and further treatment, their condition and the permissible route for disposal must be professionally clarified. For assembled modules without glass breakage, however, it is crucial whether they are functional and actually intended for reuse. The legal and practical demarcation is explained in the SecondSol contribution Used PV Modules when is a solar module used goods and when waste.

Conclusion

Sudden glass breakage is not an inexplicable random event, but often the result of several interacting factors. Thin glass can be technically sound; large module areas, local frame contacts, low mechanical reserves, pre-damage, and the actual installation can, however, increase the risk.

 

For operators, this means three steps: systematically record damages, professionally assess the electrical and mechanical safety, and jointly inspect modules and substructures when there are accumulations. A passed type test or an initially normal yield does not replace this assessment.

Frequently Asked Questions

Can a glass module break without hail or impact?

Yes. A fracture can arise from existing edge or surface damage, low glass tension, local contact points, as well as stresses from frame, embedding, and mounting. However, the cause should not be determined as spontaneous or material-based without investigation.

Are all modules with 2 millimeter glass particularly endangered?

No. 2.0-millimeter glass can be fully thermally pre-stressed, and the large majority of corresponding systems show no noticeable fracture rates. The glass thickness is only one factor within the entire module and mounting design.

Does a passed IEC test prove long-term fracture safety?

The IEC type-testing is an important minimum requirement, but it cannot fully capture rare statistical glass defects or any project-specific module substructure combination. Extended tests with larger samples can provide additional security.

May a broken module be operated if it still delivers power?

No safe clearance can be derived from the yield alone. Glass fracture can affect moisture protection, insulation, and mechanical stability. An electrical expert should decide on decommissioning and replacement.

Can broken module glass be repaired?

A permanent repair that restores the original certified module layout is generally not possible in the field. Provisional bonding neither replaces mechanical strength nor electrical insulation and long-term sealing.

Which test shows the cause of the glass fracture?

There is usually no single testing procedure. Fracture pattern, mounting, frame contacts, series patterns, electrical tests, and if necessary, laboratory analyses must be considered together. Electroluminescence shows possible cell damage but does not automatically prove the cause of the fracture.